都说某拓质量好,接杯下地一箱油就磨成这样是我想不到的
刚保养完,换了全车接杯,下地一箱油就磨成这样了,无语!http://image.rcfans.com/pic/20230904/1693820780309367_670.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
http://image.rcfans.com/pic/20230904/169382096538921_124.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
中7k,前5k,后3k,30.5的动力,都是很正常的配置,这样的异常磨损真的让人头大 这个是我是不信的 看我不揍你 发表于 2023-09-04 18:06
这个是我是不信的
呵呵
http://image.rcfans.com/pic/20230904/169382263151474_742.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
http://image.rcfans.com/pic/20230904/1693822637477504_706.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
http://image.rcfans.com/pic/20230904/1693822644080585_796.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
http://image.rcfans.com/pic/20230904/169382265055738_638.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20 再说说售后,后差速大齿到手发现打磨痕迹,轴承装上去有虚位,售后说第二天问一下没有后续。接杯异常磨损反馈给客服显示已读,没有任何回复。就事论事而已,没有黑,没有造谣。
http://image.rcfans.com/pic/20230904/1693823600799142_890.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
http://image.rcfans.com/pic/20230904/1693823600816686_34.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
http://image.rcfans.com/pic/20230904/169382360081876_980.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20
http://image.rcfans.com/pic/20230904/1693823600817169_548.jpg?x-oss-process=image/watermark,image_cGljLzIwMjExMDA2L29zc18xNjMzNTM0ODIxOTgzXzg2NF81MzNfNTYucG5n,t_50,g_se,x_20,y_20 哎哟我了个去 放煤气灶烧然后放机油里,会好一点 把狗骨改成顶丝的,用钛合金销子,接杯磨损快肯定是销子硬没有弹性。 质量不行呀 hekun0120 发表于 2023-09-05 00:10
把狗骨改成顶丝的,用钛合金销子,接杯磨损快肯定是销子硬没有弹性。
我觉得是他这一批的东西有问题,对比之前旧的接杯这个磨损的太快了,之前论坛有人发帖说某拓的接杯很耐磨的,我现在这个接杯甚至没有某凡的耐磨,不是钢材有问题就是热处理不到位